Quote:
Originally Posted by Halcyon/Tinker View Post
No!

stop! Do not pass go!

I've had a lot of very bad experiences with ktm9 bubbling and blistering where skin touches it. Absolute nightmare. It's possible that it was the flow retarder added, or possibly the film itself, I'm not sure, I believe I had that issue with no retarder added as well, it's been a long time since those days.

KTM-SV, on the other hand, did not react that way, and was just as easy to apply and buff. Quite nice looking finish.

I'd really give the ktm9 a pass.
interesting ed,
I'm do a lot of looking on this. i THINK they changed the formula recently ... maybe to address this? I know LMII stopped carrying it a while.
Thanks for the input. I'll do research and wait on starting the finish tomorrow.