The solution you're asking about is Ferric Chloride. It dulls hardware that are nickel plated in about 10 seconds, unfortunately gold plating makes it non-reactive. That's precisely why Gotoh developed the X-Gold finish, to simulate the now popular and trendy "raw brass" hardware which has naturally aged.

This is a fairly common topic at Banjohangout.org in the building, setup, and repair forum if you want to see what else is recommended.